【摘要】:铁矿选矿厂使用脂肪酸类阴离子捕收剂反浮选铁矿物,存在捕收剂用量大、所需浮选温度高、浮选指标差等问题。东北大学研发了一种新型酰胺基羧酸捕收剂DWD-3,并应用于司家营混磁精反浮选脱硅。实验室试验结果表明,在浮选温度为25℃,粗选矿浆pH=11.5、DWD-3用量为400 g/t、CaCl_2用量为400 g/t、玉米淀粉用量为1 000 g/t时,经1粗1精3扫闭路反浮选,能获得精矿铁品位66.48%、回收率80.32%,尾矿铁品位16.35%的指标。以捕收剂DWD-3代替现场捕收剂GK-68可使浮选温度由40℃降至25℃,并且精矿铁品位提高了0.39个百分点、回收率提高了2.23个百分点,尾矿铁品位降低了1.57个百分点。对浮选产品分析表明,精矿中存在20μm以下的紧密连生体;尾矿中有大量较大颗粒连生体,且连生体中铁矿物与脉石部分相互浸染连生,是尾矿铁品位较高的原因。
[Abstract]:Iron ore concentrator uses fatty acid anion collector to reverse flotation iron minerals, which has many problems, such as large amount of collector, high flotation temperature, poor flotation index and so on. A new Amido-carboxylic acid collector DWD-3, was developed and applied to the desilication of Sijiaying mixed magnetic fine flotation. The results of laboratory test show that when the flotation temperature is 25 鈩,

本文编号:2446042

资料下载
论文发表

本文链接:https://www.wllwen.com/kejilunwen/kuangye/2446042.html


Copyright(c)文论论文网All Rights Reserved | 网站地图 |

版权申明:资料由用户24b09***提供,本站仅收录摘要或目录,作者需要删除请E-mail邮箱bigeng88@qq.com