当前位置:主页 > 科技论文 > 石油论文 >

外加厚油管加厚端常见缺陷及预防措施

发布时间:2018-12-14 04:15
【摘要】:为了提高外加厚油管加厚端质量、减少缺陷的产生,以加厚Φ73.02 mm×5.51 mm油管为例,分析了油管外加厚端外表面凸棱、结疤、管端飞边、内表面凹坑等缺陷产生的原因,并给出了相应的预防措施,主要有调整加热温度、改善润滑冷却效果、保证钢管送料位置等措施,可减少内表面凹坑和外表面结疤等缺陷的出现;根据加厚缩短量计算公式计算出理论缩短量,进而确定冲头行程,能有效减少端面凹槽、内凹坑缺陷的产生。
[Abstract]:In order to improve the quality of thickened tubing and reduce the production of defects, taking the thickened 桅 73.02 mm 脳 5.51 mm tubing as an example, the causes of the defects such as convex edges, scarring, flying edges at the end of the tubing and pits on the inner surface are analyzed. The corresponding preventive measures are given, such as adjusting the heating temperature, improving the lubricating and cooling effect, ensuring the feeding position of the steel pipe, and so on, which can reduce the appearance of the inner surface pit and the outer surface scar and so on. The theoretical shortening is calculated according to the formula of thickening shortening, and then the stroke of punching head is determined, which can effectively reduce the appearance of the defects in the end groove and the inner pit.
【作者单位】: 宝鸡石油钢管有限责任公司西安石油专用管分公司;
【分类号】:TE931.2

【相似文献】

相关期刊论文 前4条

1 崔奋;张德松;王国正;张朋举;刘延成;贾美玲;;外加厚油管一次成形技术应用分析[J];石油矿场机械;2010年11期

2 商伟;中原油田胡109井砂卡3″外加厚油管事故处理工艺[J];内蒙古石油化工;2005年03期

3 张广路;杨鹏;韩军;;φ89mmAPI外加厚油管接头上扣扭矩实验研究[J];钻采工艺;2012年01期

4 ;[J];;年期

相关重要报纸文章 前1条

1 特约记者 魏世华邋记者 罗建东;“吐哈制造”叫响市场[N];中国石油报;2007年



本文编号:2377904

资料下载
论文发表

本文链接:https://www.wllwen.com/kejilunwen/shiyounenyuanlunwen/2377904.html


Copyright(c)文论论文网All Rights Reserved | 网站地图 |

版权申明:资料由用户32672***提供,本站仅收录摘要或目录,作者需要删除请E-mail邮箱bigeng88@qq.com