【摘要】:以含铁量较高的矿物原料引入铁元素,在梭式窑1310℃还原气氛下,制得翠绿透明的裂纹梅子青釉。实验选择釉果、釉灰、石英、煅烧高岭土进行单因素试验,探讨了其对梅子青釉光泽度、气泡、针孔、裂纹、外观呈色及色度值的影响,在此基础上,对裂纹梅子青釉配方进行了正交试验优化,得出最优配方。
[Abstract]:The green and transparent cracked plum green glaze was prepared by introducing iron element into mineral material with high iron content and reducing atmosphere at 1310 鈩,