基于工作性能的纤维纳米混凝土配合比设计方法
发布时间:2019-05-10 03:43
【摘要】:采用基于工作性能的纤维纳米混凝土配合比设计方法,测定了纳米材料和钢纤维体积率对水泥浆体富余系数和砂浆富余系数的影响,提出了纤维纳米混凝土的最优配合比.结果表明,该方法具有试验量小、适用性广的优点,能为纤维纳米混凝土的工程应用提供参考.
[Abstract]:The influence of nano-material and steel fiber volume ratio on the surplus coefficient of cement paste and mortar was measured by using the design method of fiber nano-concrete mix ratio based on working performance. The optimum mix ratio of fiber nano-concrete was put forward. The results show that the method has the advantages of small test quantity and wide applicability, and can provide reference for the engineering application of fiber nanoconcrete.
【作者单位】: 郑州大学新型建材与结构研究中心;湖北水总水利水电建设股份有限公司;
【基金】:国家自然科学基金(51178434)
【分类号】:TU528.572
,
本文编号:2473314
[Abstract]:The influence of nano-material and steel fiber volume ratio on the surplus coefficient of cement paste and mortar was measured by using the design method of fiber nano-concrete mix ratio based on working performance. The optimum mix ratio of fiber nano-concrete was put forward. The results show that the method has the advantages of small test quantity and wide applicability, and can provide reference for the engineering application of fiber nanoconcrete.
【作者单位】: 郑州大学新型建材与结构研究中心;湖北水总水利水电建设股份有限公司;
【基金】:国家自然科学基金(51178434)
【分类号】:TU528.572
,
本文编号:2473314